Title: Effect of Algae Infested Water on the Strength of Concrete

Author(s): Benjamin C. Doell

Publication: Journal Proceedings

Volume: 51

Issue: 12

Appears on pages(s): 333-342

Keywords: no keywords

DOI: 10.14359/11681

Date: 12/1/1954

Abstract:
The purpose of this study was to establish a relationship between loss in strength of concrete and various concentrations of organic matter contained in algae infested water. Various amounts were added to the mixing water of test batched with the resluting cylinders tested at 28 and 60 days. A close approximation of the allowable concentration of organic matter in a good mixing water was established.




  