Title: Future-Proofing Concrete: How to Prolong Your Concrete’s Lifespan

Author(s): Jennifer K. Mizer

Publication: Concrete International

Volume: 47

Issue: 1

Appears on pages(s): 34-36

Keywords: material, technology, impact, practice

DOI:

Date: 1/1/2025

Abstract:
The longevity of concrete is influenced by several interrelated challenges, each contributing to its gradual degradation. By addressing both technical and environmental considerations, stakeholders can achieve durable, cost-effective, and eco-friendly concrete solutions that contribute to the long-term sustainability of concrete.




  