Vibration Performance of Inter-Module Composite Floors for Modular Buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Vibration Performance of Inter-Module Composite Floors for Modular Buildings

Author(s): Youjin Chae, Min-Jun Jeon, Chang-Kil Ju, Seung-Il Kim, and Tae-Sung Eom

Publication: Symposium Paper

Volume: 364

Issue:

Appears on pages(s): 20-39

Keywords: modular construction, floor vibration, composite structure, precast concrete, serviceability

DOI: 10.14359/51745454

Date: 12/1/2024

Abstract:
Modular construction has been attracting attention worldwide as a promising solution to reduce construction time and labor demand. In this study, a new inter-module composite floor system that connects the upper module floor beams and lower module ceiling beams was experimentally and analytically investigated with an emphasis on vibration performance under service loading. First, the upper module floor of 2 m [6.56 ft] wide and 6 m [19.7 ft] long was fabricated as a composite system consisting of precast concrete (PC) panels, steel beams and ultra high-performance concrete (UHPC) connectors. Structural integrity between PC panels, steel beams and UHPC connectors were secured using grouting and topping mortar. Then, the lower module ceiling beams were connected to the upper module floor beams by fully tensioned high-tension bolts (i.e., slip-critical connection) to complete the inter-module composite floor. The vibration frequencies, damping ratio, and acceleration responses of the inter-module composite floors were measured from laboratory tests such as impact hammer, heel drop and walking tests, considering the number and location of the connecting bolts as the test parameter. The vibration characteristics of the inter-module composite floors were investigated further through finite element analysis. The measured and predicted vibration performances were compared with the acceptance criteria in AISC Design Guide 11 and ISO 10137.

Related References:

1. Murray, T. M., Allen, D. E., Ungar, E. E., & Davis, B. D. (2016). Vibrations of Steel Framed Structural Systems Due to Human Activity. Design Guide Series 11 (AISC DG11), Second Edition. American Institute of Steel Construction

2. ISO (2007), Bases for Design of Structures – Serviceability of Building against Vibration. ISO 10137. International Organization for Standardization.

3. CSA, 1989, Canadian Standard: Steel Structures for Buildings - Limits States Design: Appendix G, Guide for Floor Vibration, CAN3 -S16.1 -M89, Rexdale, Ontario.

4. Smith, A.L., Hicks, S.J., and Devine, P.J. (2009) Design of Floors for Vibration: A New Approach (Revised Edition). SCI P354. The Steel Construction Institute. Berkshire, UK.

5. Chen, Z., Liu, J., Yu, Y., Zhou, C., & Yan, R. (2017). Experimental study of an innovative modular steel building connection. Journal of Constructional Steel Research, 139, 69–82. doi: 10.1016/j.jcsr.2017.09.008

6. Khan, K. and Yan, J.-B. (2020). Finite Element Analysis on Seismic Behaviour of Novel Joint in Prefabricated Modular Steel Building. International Journal of Steel Structures, 20(3), 752–765. doi: 10.1007/s13296-020-00320-w

7. Lacey, A.W., Chen, W., Hao, H., and Bi, K. (2021). New Interlocking Inter-Module Connection for Modular Steel Buildings: Simplified Structural Behaviours. Engineering Structures, 227, 111409. doi: 10.1016/j.engstruct.2020.111409

8. Chen, Z., Wang, J., Liu, J., and Khan, K. (2021). Seismic Behavior and Moment Transfer Capacity of an Innovative Self-Locking Inter-Module Connection for Modular Steel Building. Engineering Structures, 245, 112978. doi: 10.1016/j.engstruct.2021.112978

9. Srisangeerthanan, S., Hashemi, M.J., Rajeev, P., Gad, E., and Fernando, S. (2020). Review of Performance Requirements for Inter-Module Connections in Multi-Story Modular Buildings. Journal of Building Engineering, 28, 101087. doi: 10.1016/j.jobe.2019.101087

10. Celin, M.A.M. (2023). Vibration Serviceability Assessment of a Steel Modular Floor System. MS Thesis. Virginia Tech. Blacksburg, Virginia.

11. ABAQUS Analysis user’s manual 6.10-EF (2010) Dassault systems Simulia corp., Providence, RI, USA

12. DIANA. Finite element analysis, release 10.8. TNO building and construction research. Delft, Netherlands. 2024.

13. MIDAS-GEN. Gen 2024 On-line Manual. MIDAS Information Technology Co., Ltd. (https://manual.midasuser.com/KR/Gen/945/MidasGen.htm)

14. Bachmann, H., Lively Footbridges – a real challenge, Footbridge 2002 – Design and dynamic behavior of Footbridges, 2002