Title:
Shear Strength and Model of Non-prestressed Rectangular UHPC Beams: Influence of Coarse Aggregate
Author(s):
Kuo-Wei Wen, Manuel Bermudez, and Chung-Chan Hung
Publication:
Symposium Paper
Volume:
363
Issue:
Appears on pages(s):
94-117
Keywords:
UHPC, coarse aggregate, shear strength, shear span-to-depth ratio, shear strength model
DOI:
10.14359/51742109
Date:
7/1/2024
Abstract:
Ultra-high-performance concrete (UHPC) features tensile strain-hardening behavior and a high compressive strength. Existing studies on the shear behavior of UHPC structural members have been focused on prestressed UHPC girders. More experimental data of the shear behavior of non-prestressed UHPC beams are necessary to quantify the safety margin of shear designs for structures. Moreover, while the UHPC members in most studies did not contain coarse aggregate to strengthen their microstructure, the inclusion of coarse aggregate has been shown to substantially reduce the autogenous shrinkage and enhance the elastic modulus for UHPC materials, which is beneficial for structural applications of UHPC. This study experimentally investigated the shear failure behavior of eighteen non-prestressed rectangular UHPC beams. The experimental variables included the volume fraction of fibers, shear span-to-depth ratio of the beams, and coarse aggregate. The detailed shear failure responses of the UHPC beams were discussed in terms of the damage pattern, shear modulus, shear strength, shear strain, and strain energy. The test results showed that the inclusion of coarse aggregate increased the beam shear strength, and its enhancement became more significant with a higher volume fraction of fibers and a lower shear span-to-depth ratio of the beam. In addition to the experimental investigation, a shear strength model for non-prestressed rectangular UHPC beams that accounts for the interactive effect of the key design parameters was developed. An experimental database of the shear strength of the UHPC beams in existing studies was established to assess the performance of the proposed model. It was shown that the proposed model reasonably predicted the shear strength of the UHPC beams in the database with a higher accuracy and lower scatter compared to the results of existing models.
Related References:
1. Richard, P. and M. Cheyrezy, Composition of reactive powder concretes. Cement and concrete research, 1995.25(7): p. 1501-1511.
2. Rossi, P., A. Arca, E. Parant, and P. Fakhri, Bending and compressive behaviours of a new cement composite.Cement and Concrete Research, 2005. 35(1): p. 27-33.
3. Farhat, F., D. Nicolaides, A. Kanellopoulos, and B.L. Karihaloo, High performance fibre-reinforced cementitiouscomposite (CARDIFRC)–Performance and application to retrofitting. Engineering fracture mechanics, 2007. 74(1-2):p.151-167.
4. Wille, K., A.E. Naaman, and G.J. Parra-Montesinos, Ultra-High Performance Concrete with Compressive StrengthExceeding 150 MPa (22 ksi): A Simpler Way. ACI materials journal, 2011b. 108(1).
5. Wille, K., D.J. Kim, and A.E. Naaman, Strain-hardening UHP-FRC with low fiber contents. Materials andstructures, 2011a. 44(3): p. 583-598.
6. Park, S.H., D.J. Kim, G.S. Ryu, and K.T. Koh, Tensile behavior of ultra high performance hybrid fiber reinforcedconcrete. Cement and Concrete Composites, 2012. 34(2): p. 172-184.
7. Aghdasi, P., A.E. Heid, and S.-H. Chao, Developing Ultra-High-Performance Fiber-Reinforced Concrete for Large-Scale Structural Applications. ACI Materials Journal, 2016. 113(5).
8. Alkaysi, M. and S. El-Tawil, Effects of variations in the mix constituents of ultra high performance concrete(UHPC) on cost and performance. Materials and Structures, 2016. 49(10): p. 4185-4200.
9. Hung, C.-C., Y.-T. Chen, and C.-H. Yen, Workability, fiber distribution, and mechanical properties of UHPC withhooked end steel macro-fibers. Construction and Building Materials, 2020. 260: p. 119944.
10. Hung, C.-C. and P.-L. Hsieh. Comparative study on shear failure behavior of squat high-strength steel reinforcedconcrete shear walls with various high-strength concrete materials. in Structures. 2020. Elsevier.
11. Shao, Y., C.-C. Hung, and S.L. Billington, Gradual crushing of steel reinforced HPFRCC beams: Experimentsand simulations. J. Struct. Eng, 2021. 147(8): p. 04021114.
12. Graybeal, B., Design and construction of field-cast UHPC connections. 2014, United States. Federal HighwayAdministration.
13. Graybeal, B.A., Material property characterization of ultra-high performance concrete. 2006, United States.Federal Highway Administration. Office of Infrastructure.
14. Al-Osta, M., M. Isa, M. Baluch, and M. Rahman, Flexural behavior of reinforced concrete beams strengthenedwith ultra-high performance fiber reinforced concrete. Construction and Building Materials, 2017. 134: p. 279-296.
15. Hung, C.-C., H. Li, and H.-C. Chen, High-strength steel reinforced squat UHPFRC shear walls: Cyclic behaviorand design implications. Engineering Structures, 2017. 141: p. 59-74.
16. Hung, C.-C., F.-Y. Hu, and C.-H. Yen, Behavior of slender UHPC columns under eccentric loading. EngineeringStructures, 2018. 174: p. 701-711.
17. Hung, C.C., H.S. Lee, and S.N. Chan, Tension-stiffening effect in steel-reinforced UHPC composites:Constitutive model and effects of steel fibers, loading patterns, and rebar sizes. Composites Part B: Engineering, 2019.158: p. 269-278.
18. Chan, T., K.R. Mackie, and Z.B. Haber, Precast Seismic Bridge Column Connection Using Ultra-High-Performance Concrete Lap Splice. ACI Structural Journal, 2020. 117(1).
19. Shao, Y., C.-W. Kuo, and C.-C. Hung, Seismic performance of full-scale UHPC-jacket-strengthened RC columnsunder high axial loads. Engineering Structures, 2021. 243: p. 112657.
20. Hung, C.-C., C.-W. Kuo, and Y. Shao, Cast-in-place and prefabricated UHPC jackets for retrofitting shear-deficient RC columns with different axial load levels. Journal of Building Engineering, 2021. 44: p. 103305.
21. Karmacharya, A. and S.-H. Chao. Precast ultra-high-performance fiber-reinforced concrete (UHP-FRC) for fastand sustainable pavement repair. in MATEC Web of Conferences. 2019. EDP Sciences.
22. Tazarv, M. and M.S. Saiidi, UHPC-filled duct connections for accelerated bridge construction of RC columns inhigh seismic zones. Engineering Structures, 2015. 99: p. 413-422.
23. El-Tawil, S., Y.-S. Tai, B. Meng, W. Hansen, and Z. Liu, Commercial production of non-proprietary ultra highperformance concrete. 2018, Michigan. Dept. of Transportation. Research Administration.
24. De la Varga, I., Z. Haber, and B. Graybeal, Enhancing shrinkage properties and bond performance of prefabricatedbridge deck connection grouts: material and component testing. Journal of Materials in Civil Engineering, 2018. 30(4):p.04018053.
25. Hung, C.-C., S. El-Tawil, and S.-H. Chao, A review of developments and challenges for UHPC in structuralengineering: Behavior, analysis, and design. Journal of Structural Engineering, 2021. 147(9): p. 03121001.
26. Voo, Y.L., W.K. Poon, and S.J. Foster, Shear strength of steel fiber-reinforced ultrahigh-performance concretebeams without stirrups. Journal of structural engineering, 2010. 136(11): p. 1393-1400.
27. Morcous, G., M. Maguire, and M. Tadros, Shear capacity of ultra-high-Performance concrete I-girders withorthogonal welded wire reinforcement. Special Publication, 2009. 265: p. 511-532.
28. Russell, H.G., B.A. Graybeal, and H.G. Russell, Ultra-high performance concrete: A state-of-the-art report forthe bridge community. 2013, United States. Federal Highway Administration. Office of Infrastructure ….
29. AASHTO, AASHTO LRFD Bridge Design Specifications, 4th edition. 2007, American Association of StateHighway and Transportation Officials,: Washington, DC.
30. Baby, F., P. Marchand, and F. Toutlemonde, Shear behavior of ultrahigh performance fiber-reinforced concretebeams. I: Experimental investigation. Journal of structural engineering, 2014. 140(5): p. 04013111.
31. Baby, F., P. Marchand, and F. Toutlemonde, Shear behavior of ultrahigh performance fiber-reinforced concretebeams. II: Analysis and design provisions. Journal of structural engineering, 2014. 140(5): p. 04013112.
32. AFGC-SETRA, Ultra High Performance Fibre-Reinforced Concretes. Interim recommendations, 2002.
33. Lim, W.-Y. and S.-G. Hong, Shear tests for ultra-high performance fiber reinforced concrete (UHPFRC) beamswith shear reinforcement. International Journal of Concrete Structures and Materials, 2016. 10(2): p. 177-188.
34. Pansuk, W., T.N. Nguyen, Y. Sato, J. Den Uijl, and J. Walraven, Shear capacity of high performance fiberreinforced concrete I-beams. Construction and Building Materials, 2017. 157: p. 182-193.
35. Yousef, A.M., A.M. Tahwia, and N.A. Marami, Minimum shear reinforcement for ultra-high performance fiberreinforced concrete deep beams. Construction and Building Materials, 2018. 184: p. 177-185.
36. Pourbaba, M., A. Joghataie, and A. Mirmiran, Shear behavior of ultra-high performance concrete. Constructionand Building Materials, 2018. 183: p. 554-564.
37. Mészöly, T. and N. Randl, Shear behavior of fiber-reinforced ultra-high performance concrete beams. EngineeringStructures, 2018. 168: p. 119-127.
38. Bermudez, M., K.-W. Wen, and C.-C. Hung, A Comparative Study on the Shear Behavior of UHPC Beams withMacro Hooked-End Steel Fibers and PVA Fibers. Materials, 2022. 15(4): p. 1485.
39. El-Helou, R.G. and B.A. Graybeal, Shear Behavior of Ultrahigh-Performance Concrete Pretensioned BridgeGirders. Journal of Structural Engineering, 2022. 148(4): p. 04022017.
40. Randl, N., T. Mészöly, and P. Harsányi, Shear behaviour of UHPC beams with varying degrees of fibre and shearreinforcement, in High tech concrete: Where technology and engineering meet. 2018, Springer. p. 500-507.
41. ACI Committee 318, "Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,"American Concrete Institute, Farmington Hill, MI, 520 pp.
42. CEN. Eurocode 2: Design of concrete structures - Part 1: General rules and rules for buildings. EN1992-1-1.Brussels; 2004.
43. Korean Concrete Institute, Concrete structure design code (KCI 2012), Korean Concrete Institute, Seoul (2012).
44. AFGC and SETRA. Ultra-High Performance Fibre Reinforced Concrete-Interim Recommendations. France;2013.
45. Yu, Z., L. Wu, Z. Yuan, C. Zhang, and T. Bangi, Mechanical properties, durability and application of ultra-high-performance concrete containing coarse aggregate (UHPC-CA): A review. Construction and Building Materials, 2022.334: p. 127360.
46. Li, S., O.M. Jensen, Z. Wang, and Q. Yu, Influence of micromechanical property on the rate-dependent flexuralstrength of ultra-high performance concrete containing coarse aggregates (UHPC-CA). Composites Part B:Engineering, 2021. 227: p. 109394.
47. Zeng, X., K. Deng, H. Liang, R. Xu, C. Zhao, and B. Cui, Uniaxial behavior and constitutive model ofreinforcement confined coarse aggregate UHPC. Engineering Structures, 2020. 207: p. 110261.
48. Ma, J., M. Orgass, F. Dehn, D. Schmidt, and N. Tue. Comparative investigations on ultra-high performanceconcrete with and without coarse aggregates. in International Symposium on Ultra High Performance Concrete, Kassel,Germany. 2004.
49. Mazanec, O. and P. Schießl. Mixing time optimisation for UHPC. in Proceedings of the second internationalsymposium on ultra high performance concrete, Kassel. 2008.
50. ASTM A615/A615M.Standard Specification for Deformed and Plain Carbon-Steel Bars for ConcreteReinforcement. 2020.
51. ASTM C172/C172M. Standard Practice for Sampling Freshly Mixed Concrete.
52. ASTM C31/C31M. Standard Practice for Making and Curing Concrete Test Specimens in the Field.
53. ASTM C39/C39M. Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens.
54. Athanasopoulou, A., Shear strength and drift capacity of reinforced concrete and high-performance fiberreinforced concrete low-rise walls subjected to displacement reversals. 2010, University of Michigan.
55. ASTM C1856/C1856M. Standard practice for fabricating and testing specimens of ultra-high performanceconcrete. West Conshohocken, PA: ASTM. 2017.
56. CSA (Canadian Standards Association) Concrete materials and methods of concrete construction/test methodsand standard practices for concrete. A23.1:19/A23.2:19. Toronto: CSA. 2019.
57. Naaman, A.E. and K. Wille, The path to ultra-high performance fiber reinforced concrete (UHP-FRC): fivedecades of progress. Proceedings of Hipermat, 2012: p. 3-15.
58. CSA A23.3-14, “Design of Concrete Structures,” Canadian Standards Association, Mississauga, ON, Canada,2014, 297 pp.
59. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.
60. Fenwick, R. and T. Paulay, Mechanisms of shear resistance of concrete beams. Journal of the Structural Division,1968. 94(10): p. 2325-2350.
61. ASTM C469/C469M. Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete inCompression.
62. Hung, C.C., T.Y. Yuen, C.W. Huang, and C.H. Yen, Tension lap splices in UHPC beams: Influence of rebar size,steel fibers, splice length, and coarse aggregate. Journal of Building Engineering, 2022. 55: p. 104716.
63. Graybeal, B. and M. Davis, Cylinder or cube: strength testing of 80 to 200 MPa (11.6 to 29 ksi) ultra-high-performance fiber-reinforced concrete. ACI Materials Journal, 2008. 105(6): p. 603.
64. Narayanan, R. and I. Darwish, Use of steel fibers as shear reinforcement. Structural Journal, 1987. 84(3): p. 216-227.
65. Kwak, Y.-K., M.O. Eberhard, W.-S. Kim, and J. Kim, Shear strength of steel fiber-reinforced concrete beamswithout stirrups. ACI Structural journal, 2002. 99(4): p. 530-538.
66. Gandomi, A., A. Alavi, and G. Yun, Nonlinear modeling of shear strength of SFRC beams using linear geneticprogramming. Structural Engineering and Mechanics, 2011. 38(1): p. 1-25.
67. Arslan, G., Shear strength of steel fiber reinforced concrete (SFRC) slender beams. KSCE Journal of CivilEngineering, 2014. 18(2): p. 587-594.
68. Qi, J., Z.J. Ma, and J. Wang, Shear strength of UHPFRC beams: Mesoscale fiber-matrix discrete model. Journalof Structural Engineering, 2017. 143(4): p. 04016209.
69. Sarveghadi, M., A.H. Gandomi, H. Bolandi, and A.H. Alavi, Development of prediction models for shear strengthof SFRCB using a machine learning approach. Neural Computing and Applications, 2019. 31(7): p. 2085-2094.
70. Wang, Q., H.-L. Song, C.-L. Lu, and L.-Z. Jin. Shear performance of reinforced ultra-high performance concreterectangular section beams. in Structures. 2020. Elsevier.
71. Yang, J., J.-H. Doh, K. Yan, and X. Zhang, Experimental investigation and prediction of shear capacity for UHPCbeams. Case Studies in Construction Materials, 2022. 16: p. e01097.
72. Yavaş, A., U. Hasgul, K. Turker, and T. Birol, Effective fiber type investigation on the shear behavior of ultrahigh-performance fiber-reinforced concrete beams. Advances in Structural Engineering, 2019. 22(7): p. 1591-1605.
73. Bermudez, M., & Hung, C. C. Shear behavior of ultra-high performance hybrid fiber reinforced concrete beams.In International Interactive Symposium on Ultra-High Performance Concrete (Vol. 2, No. 1). Iowa State UniversityDigital Press. 2019.