Abstract:
The decarbonization of the cement industry will require a versatile portfolio of different alternative cements. In contrast to other known and popular alternatives, cement based on MgO-rich hydrates remains an unexplored topic and little is known about the formation and stability of Mg-Al LDH as the main binding phase in a cement. In this work, we report on experimental work on the phase assemblage of MgO-Al2O3-(SiO2)-CO2-H2O system via the hydration of an amorphous magnesium aluminate (AMA) in the presence of different magnesium carbonates and metakaolin. The data reveal that hydrotalcite is the main hydrate of the cement with relatively fast reaction kinetics in which AMA is fully hydrated after 7 days of curing in ambient water. Additionally, a more detailed phase assemblage will be beneficial in the better understanding and in improving the thermodynamic data for the MgO-Al2O3-(SiO2)-CO2-H2O system and of interest to shed light on the long-term stability of this cement.
Related References:
1. E. Bernard, H. Nguyen, S. Kawashima, B. Lothenbach, H. Manzano, J. Provis, A. Scott, C. Unluer, F. Winnefeld, P. Kinnunen, MgO-based cements – Current status and opportunities, RILEM Tech. Lett. 8 (2023) 65–78. doi: 10.21809/rilemtechlett.2023.177
2. S.J. Mills, A.G. Christy, J.-M.R. Génin, T. Kameda, F. Colombo, Nomenclature of the hydrotalcite supergroup: natural layered double hydroxides, Mineral. Mag. 76 (2012) 1289–1336. doi: 10.1180/minmag.2012.076.5.10
3. H. Zhao, T. Hanein, N. Li, A. Alotaibi, A. Li, S. Walling, H. Kinoshita, Acceleration of M-S-H gel formation through the addition of alkali carbonates, in: Proc. 15th Int. Congr. Chem. Cem. ICCC 2019, Prague, Czech Republic, 2019.
4. E. Bernard, B. Lothenbach, D. Rentsch, A. German, F. Winnefeld, Effect of carbonates on the formation of magnesium silicate hydrates, Mater. Struct. 55 (2022) 183. doi: 10.1617/s11527-022-02018-3
5. E. Kanezaki, Thermal behavior of the hydrotalcite-like layered structure of Mg and Al-layered double hydroxides with interlayer carbonate by means of in situ powder HTXRD and DTA/TG, Solid State Ion. 106 (1998) 279–284. doi: 10.1016/S0167-2738(97)00494-3
6. L.A. Hollingbery, T.R. Hull, The thermal decomposition of huntite and hydromagnesite—A review, Thermochim. Acta 509 (2010) 1–11. doi: 10.1016/j.tca.2010.06.012
7. E. Bernard, B. Lothenbach, C. Cau-Dit-Coumes, I. Pochard, D. Rentsch, Aluminum incorporation into magnesium silicate hydrate (M-S-H), Cem. Concr. Res. 128 (2020) 105931. doi: 10.1016/j.cemconres.2019.105931