Title: Concrete Q&A: Measuring Flatness of Elevated Floors

Author(s):

Publication: Concrete International

Volume: 46

Issue: 6

Appears on pages(s): 75-76

Keywords: slab, straightedge, compliance, finishing

DOI:

Date: 6/3/2024

Abstract:
This month's Q&A focuses on requirements for checking flatness of suspended slabs. It discusses the time limit for measuring floor flatness after finishing, compliance requirements for the manual straightedge method, minimum number of samples, and sample distribution, as well as possible remedies for noncompliance.




  