Title: Overcoming Barriers to Adopting Carbon Reduction in Concrete

Author(s): Lawrence Sutter, Douglas Hooton, Sarah Lopez, Thomas Van Dam, Al Innis, and Kevin Senn

Publication: Concrete International

Volume: 45

Issue: 11

Appears on pages(s): 49-52

Keywords: industry, material, cement, training

DOI:

Date: 11/1/2023

Abstract:
A report was submitted to the Breakthrough Energy Foundation in April 2023 that discussed carbon reduction strategies for concrete; cement and concrete codes, specifications, and standards; current sustainability codes; risks in concrete construction; and materials production. This article summarizes the action plan provided in the conclusion of the report.




  