Shining a New Light on the Riddle of Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shining a New Light on the Riddle of Shear

Author(s): Jack J. Poldon, Neil A. Hoult, and Evan C. Bentz

Publication: Concrete International

Volume: 45

Issue: 2

Appears on pages(s): 17-25

Keywords: strain, reinforcement, design, sensor

DOI:

Date: 2/1/2023

Abstract:
The article examines the assumptions in the ACI 318 Code and design approaches for shear using the results from beam tests with varying shear reinforcement designs measured with emerging sensor technologies. It describes the research campaign, presents the distributed measurements with a discussion of the key insights, and offers some takeaways for designers.




  