ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: NEx insights
Author(s):
Publication: Concrete International
Volume: 44
Issue: 12
Appears on pages(s): 24-25
Keywords:
DOI:
Date: 12/1/2022
Abstract: Nonmetallic polymer-based materials are being increasingly deployed across multiple industries and offer new possibilities for construction. NEx was established to accelerate the use of nonmetallic materials and products in the building and construction sector.