Vapor Pressure Modeling of High-Strength Concrete at High Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Vapor Pressure Modeling of High-Strength Concrete at High Temperatures

Author(s): Jie Zhao, Jian-Jun Zheng, Gai-Fei Peng, and Meng-Qi Wang

Publication: Materials Journal

Volume: 119

Issue: 2

Appears on pages(s): 131-140

Keywords: high-strength concrete; high temperature; modeling; spalling; vapor pressure

DOI: 10.14359/51734441

Date: 3/1/2022

Abstract:
High-strength concrete (HSC) is susceptible to spalling at high temperatures. One reason for this is that vapor pressure builds up in concrete and plays a key role in spalling under certain conditions. However, vapor pressure modeling is still insufficient so far. Steam tables, which bear the actual states of water steam, have never been applied in vapor pressure modeling. In this paper, a meso-scale vapor pressure modeling approach using steam tables is presented. The effects of the thermal decomposition of the cement paste matrix and the vapor phase transfer driven by the gradient of vapor pressure are considered. By applying the theory of poromechanics, the Biot modulus is deduced and the mechanical effect of vapor pressure is modeled. Finally, the distribution and mechanical effect of vapor pressure in a 100 mm (3.94 in.) HSC cube specimen exposed to fire are modeled, and the applicability and effectiveness of the model are presented.