Title: Formwork Produced Using Additive Manufacturing

Author(s):

Publication: Concrete International

Volume: 43

Issue: 6

Appears on pages(s): 48-49

Keywords: computer-aided design, formwork, 3-D printing, precast

DOI:

Date: 6/1/2021

Abstract:
The conversion of a historic brewery in Bavaria, Germany, into an office and events space posed a challenge: the need to replace five large stone window frames while retaining the original aesthetic of the façade. Using computer-aided design files specifying the geometry of the window frames, digital patterns were created to print polymer formwork elements that were successfully used to cast the window frame elements.




  