Title: Performance of TRM/TRC systems under elevated temperatures and fire conditions
Author(s): Catherine (Corina) Papanicolaou and Thanasis Triantafillou
Publication: Symposium Paper
Volume: 345
Issue:
Appears on pages(s): 32-46
Keywords: TRM, TRC, elevated/high temperatures, fire
Date: 2/1/2021
Abstract:
In this paper, authors draw information from previous work aiming at contributing to: (i) a summary of the
existing knowledge on the mechanical performance of TRM/TRC systems under elevated temperatures and fire
conditions; and (ii) highlighting the most important issues of testing procedures and protocols. The paper refers to
both TRM- and TRC-related data. The former include experimental assessments of the: (a) TRM-to-substrate residual
bond characteristics as a function of temperature; and (b) structural performance of fired masonry elements furnished
with a new type of TRM-based overlay for combined structural and energy upgrading. TRC-related data focus on the
structural degradation of thin TRC plates under both standard and non-standard fire conditions.