Title: Two Discussions from the September 2019 ACI Materials Journal

Author(s): Donald Janssen; Jianwei Huang

Publication: Materials Journal

Volume: 117

Issue: 6

Appears on pages(s): 305-308

Keywords:

Date: 11/1/2020

Abstract:
Disc. 116-M73/From the September 2019 ACI Materials Journal, p. 67 Durability of Concrete Mixtures Containing Supplementary Cementitious Materials in Rapid Chloride Permeability Test. Paper by M. Moini, K. Sobolev, I. Flores-Vivian, S. Muzenski, L.T. Pham, S. Cramer and M. Beyene Disc. 117-M03/From the January 2020 ACI Materials Journal, p. 25 Discussion on Problem of Standard Deviation of Concrete Strength. Paper by Dai Zhenchao


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Please enter this 5 digit unlock code on the web page.