Title: Overview of Torsion Design Methods

Author(s): Camilo Granda Valencia and Eva Lantsoght

Publication: Symposium Paper

Volume: 344

Issue:

Appears on pages(s): 1-29

Keywords: codes, concrete, reinforcement, shear, torsion

Date: 10/1/2020

Abstract:
Large torsional moments, which need to be considered in a design, can result among others, in structures with an asymmetric layout or loading. To find the required longitudinal and transverse reinforcement to resist these torsional moments, the link between the three-dimensional action of the torsional moment and sectional analysis methods is necessary. This paper reviews the existing methods and code provisions for torsion. First, an overview of the principles of torsion from the mechanics perspective is given. Then, a survey of the available mechanical models for torsion is presented. Finally, the code provisions for torsion of ACI 318-19, CSA-A23.3-04, AASHTO-LRFD- 17, EN 1992-1-1:2004, and the fib Model Code 2010 are summarized. Additionally, current research topics on torsion in structural concrete are summarized. It is expected that with this paper, engineers will have a useful overview and background knowledge for the design and assessment of torsion-critical elements.




  

Please enter this 5 digit unlock code on the web page.