ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Calcium Sulfoaluminate Cement

Author(s): Robert J. Thomas, Marc Maguire, Andrew D. Sorensen, and Ivan Quezada

Publication: Concrete International

Volume: 40

Issue: 4

Appears on pages(s): 65-69

Keywords: concrete, ettringite, setting, strength

Date: 4/1/2018

Abstract:
In the North American market, calcium sulfoaluminate (CSA) cement is primarily used as a rapid pavement repair material. This article provides an overview of the unique features and benefits of CSA cement, the durability of CSA cement concrete, and ongoing and potential applications within the concrete industry.




  