Title: Inclined Headed Stud Shear Reinforcement: Design and Detailing

Author(s): Amin Ghali and Ramez B. Gayed

Publication: Symposium Paper

Volume: 321

Issue:

Appears on pages(s): 11.1-11.20

Keywords: concrete; design; detailing; flat plates; headed stud shear reinforcement; inclined; punching shear.

Date: 9/29/2017

Abstract:
Assemblies of vertical headed stud shear reinforcement are extensively used in practice to resist punching of concrete slabs. Similarly, headed studs making an angle 45 degrees with slab surface can be used for the same purpose. Equations for design and detailing are presented with examples.




  