Title: Successful Design of Wet-Mix Shotcrete

Author(s): Ezgi Yurdakul, Klaus-Alexander Rieder, and Diego Granell Nebot

Publication: Concrete International

Volume: 39

Issue: 4

Appears on pages(s): 55-59

Keywords: strength, accelerator, slump, performance

Date: 4/1/2017

Abstract:
Although wet-mix shotcrete has proven to be an ideal alternative to conventional concrete in numerous applications, its further success is sometimes hindered by a few common misconceptions. The article discusses some of those fallacies and presents corresponding facts. It also explains why successful shotcreting requires consideration of all desired performance criteria and project needs.




  