Title: Shallow Embedded Anchors
Author(s): Werner Fuchs and Jan Hofmann
Publication: Concrete International
Volume: 39
Issue: 2
Appears on pages(s): 45-53
Keywords: nonstructural, cover, redundant, reinforcement
Date: 2/1/2017
Abstract:
Although ACI 318-14 provides design requirements for anchors in concrete, it does not apply to specialty inserts used for anchoring nonstructural elements. Background information is provided on the ACI 318 design procedure, shallow anchors and related parameters are discussed, and modification factors are proposed for ACI 318 design values.