Self-Healing of Cementitious Composites to Reduce High CO2 Emissions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Self-Healing of Cementitious Composites to Reduce High CO2 Emissions

Author(s): M. Sahmaran, G. Yıldırım, G. Hasıloglu Aras, S. Bahadır Keskin, O. K. Keskin, and M. Lachemi

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 93-104

Keywords: carbonation; CO2-rich environment; electrical properties; engineered cementitious composites (ECCs); self-healing

DOI: 110.14359/51689484

Date: 1/1/2017

Abstract:
Existing concrete structures worldwide are suffering from deterioration/distress. With ever-growing urban population and global warming, higher CO2 concentrations in the atmosphere are likely to further weaken the chemical stability of concrete material, and it is very important to understand how its effects will impair the material. To help moderate the harmful effects of increased CO2 concentrations, an experimental study was undertaken in which efforts were made to accelerate the capability of engineered cementitious composites (ECCs) with different pozzolanic materials (PMs) to self-heal its own damage (for example, cracks) in a CO2-rich environment. Self-healing was assessed by electrical impedance (EI) and rapid chloride permeability tests (RCPTs) on 28-day-old specimens. Experimental findings show that self-healing in a CO2-rich environment is more pronounced than it is in normal atmospheric conditions. The findings also show that PM type can be very decisive on self-healing performance in a CO2-rich environment, depending on testing method. Results suggest that proper material design can lead to the development of environmentally friendly ECC options with superior mechanical and durability characteristics.