Title: Decorative Painting on Concrete

Author(s): Sidney F. Ross

Publication: Journal Proceedings

Volume: 24

Issue: 2

Appears on pages(s): 101-103

Keywords: none

Date: 2/1/1928

Abstract:
In 1926 our firm made its initial study of decorative painting on concrete. This was described in an article written for the Architectural Record and appeared in the April, 1927, issue. For that reason it is hardly necessary to present the matter in detail, but for those who are not familiar with what we tried to accomplish a brief outline may be of interest.




  