Title: Pumice - Lightweight Aggregate

Author(s): Leslie I. Neher

Publication: Journal Proceedings

Volume: 48

Issue: 9

Appears on pages(s): 65-75

Keywords: no keywords

DOI: 10.14359/11871

Date: 9/1/1951

Abstract:
The growth of pumice production in the United States during recent years is worthy of note. Chemical and physical properties, mix design, presaturation of aggregates and the application of pumice aggregates in lightweight tilt-up and masonry construction are discussed.




  