Title: Guide for Certification of Nuclear Concrete Inspection and Testing Personnel

Author(s): ACI Committee 311

Publication: Journal Proceedings

Volume: 72

Issue: 7

Appears on pages(s): 338-346

Keywords: aggregates;concrete construction;concretes;criteria;education;inspection; nuclear reactors; personnel development;pressure vessels; qualifications; quality control;reinforcing steel;specification;standards;training courses.

Date: 7/1/1975

Abstract:
Presents a guide for the required certification of Level I Inspection technicians and Level II Inspectors performing inspection on nuclear power plants in accordance with Appendix VII of the Joint ACI-ASME Standard "Code for Concrete Reactor Vessels and Containments (ACI 359-74)." The certification of Level II Inspection Engineers is not covered in this report but is found in Appendix VII of ACI 359-74.




  