Guide for Making a Condition Survey of Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Guide for Making a Condition Survey of Concrete Pavements

Author(s): ACI Committee 201

Publication: Journal Proceedings

Volume: 83

Issue: 3

Appears on pages(s): 455-476

Keywords: airports; concrete durability concrete pavements; cracking (fracturing); highways; joints (junctions); parking facilities; serviceability; surface defects; surveys; warehouses.

DOI: 10.14359/10741

Date: 5/1/1986

Abstract:
This guide presents a method for making a condition survey of such concrete pavements as highways, airfields, parking lots, and traffic areas in warehouses. The condition survey consists of (I) an examination of the exposed concrete to identify and define areas of distress and (ii) a determination of the pavement's riding quality. Condition checklists and descriptions of various distress manifestations are included.




  