Title: Concrete Q&A: Strategies for Obtaining Low-Carbon Concrete Mixtures for Paving

Author(s):

Publication: Concrete International

Volume: 46

Issue: 11

Appears on pages(s): 111-112

Keywords: aggregate, cement, binder, performance

DOI:

Date: 11/1/2024

Abstract:
It is estimated that almost 90% of the embodied carbon emissions in a concrete mixture come from the production of portland cement. This month’s Q&A discusses strategies that can be adopted for obtaining low-carbon concrete mixtures for paving.




  