Constructability of Anchor Bolts (Rods) in Foundations

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Constructability of Anchor Bolts (Rods) in Foundations

Author(s): James E. Klinger, Eamonn F. Connolly, Charles D. Charlson, Oscar R. Antommattei, and Bruce A. Suprenant

Publication: Concrete International

Volume: 46

Issue: 7

Appears on pages(s): 38-41

Keywords: tolerance, elevation, construction, projection

DOI:

Date: 7/1/2024

Abstract:
Various codes, specifications, and reports provide different requirements/recommendations for anchor bolt (rod) installation in foundations. The article discusses the issues related to these requirements/recommendations and encourages designers to add 2 in. (50 mm) to the calculated design embedment length and to specify the elevation of the top of the anchor bolt.




  