Title: Concrete Q&A: Selecting a Protection System

Author(s):

Publication: Concrete International

Volume: 46

Issue: 5

Appears on pages(s): 80

Keywords: surface, preparation, application, manufacturer

DOI:

Date: 5/1/2024

Abstract:
To enhance or extend service life of concrete elements and structures, installation of a protection system can provide a barrier between the concrete and damage from deleterious materials or conditions. This month's Q&A discusses selection of a protection system as well as adequate surface preparation prior to application of a protection system.




  