Title: Why is Concrete Scanning Important?

Author(s): Jennifer Britt

Publication: Concrete International

Volume: 46

Issue: 4

Appears on pages(s): 43-45

Keywords: GPR, bar, thickness, conduit

DOI:

Date: 4/1/2024

Abstract:
Existing concrete slabs and structures require scanning and imaging before any build out, renovation, or excavation work begins. Ground-penetrating radar technology has established itself as the primary tool for fast, effective, and efficient determination of the presence of utilities and embedded structural members, such as post-tensioning tendons and reinforcing bars.




  