International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI-ASCC Survey on Portland-Limestone Cement Concrete

Author(s): James Klinger, Kevin A. MacDonald, Jerry A. Holland, Scott M. Tarr, Beverly A. Garnant, and Bruce A. Suprenant

Publication: Concrete International

Volume: 46

Issue: 2

Appears on pages(s): 27-36

Keywords: question, problem, floor, slab

DOI:

Date: 2/1/2024

Abstract:
A Joint ACI-ASCC Task Group developed a survey to gather information regarding the construction of concrete floors and slabs using ordinary portland cement (OPC) and portland-limestone cement. This article presents 15 survey questions and a summary of responses provided by 173 respondents, as well as information from previously conducted surveys.




  