Title: The Essence of Carbon Neutrality in Concrete- Related Technologies

Author(s): Koji Sakai and Takeju Matsuka

Publication: Concrete International

Volume: 45

Issue: 11

Appears on pages(s): 40-41

Keywords: slag, steel, fly ash, emission

DOI:

Date: 11/1/2023

Abstract:
Slag and fly ash are increasingly being used in concrete mixtures as cement replacement to reduce the use of clinker and consequently decreasing CO2 emissions. However, these by-products are generated simultaneously with the production of steel and electricity and therefore should be regarded as bearing CO2 derived from the energy necessary for their production.




  