Laser Scanning Basics for Concrete Tolerance Verification

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Laser Scanning Basics for Concrete Tolerance Verification

Author(s): Lingfeng (Leo) Zhang and John M. Russo

Publication: Concrete International

Volume: 45

Issue: 9

Appears on pages(s): 23-29

Keywords: scanner, target, data, resolution

DOI:

Date: 9/1/2023

Abstract:
The method and apparatus used to verify concrete tolerances should be capable of reliably measuring to the specified tolerance or less. The purpose of this article is to provide users with an in-depth review of the data comparison from a live laser scanning event at Geo Week 2023, as well as to help users in selecting a proper laser scanner for concrete tolerance verification.




  