Title: Concrete Q&A: Can Testing Laboratories Have True Companions?
Author(s):
Publication: Concrete International
Volume: 44
Issue: 8
Appears on pages(s): 63-64
Keywords: results, owner, producer, difference
Date: 8/1/2022
Abstract:
This month’s Q&A focuses on evaluation and comparison of test results provided by owner’s and concrete producer’s testing agencies. It discusses responsibilities of the owner’s testing agency specified in ACI 301-20 as well as acceptable differences in test results based on interlaboratory studies and precision statements provided in relevant ASTM standards.