Title: Statewide Survey of Chemically Stabilized Soil Properties for Mechanistic-Empirical Pavement Design

Author(s): A. S. Carey, L. A. Cooley Jr., A. Middleton, W. G. Sullivan, L. E. W. Ayers, and I. L. Howard

Publication: Materials Journal

Volume: 119

Issue: 5

Appears on pages(s): 227-238

Keywords: cement stabilization; chemically stabilized soil; in-place properties; lime-fly ash stabilization; lime stabilization; mechanistic-empirical pavement design

DOI: 10.14359/51735957

Date: 9/1/2022