Title: Concrete Q&A: Ties in Foundation Pedestal and Strength Test Age Requirements

Author(s):

Publication: Concrete International

Volume: 43

Issue: 11

Appears on pages(s): 96

Keywords: section, design, mixture, documents

Date: 11/1/2021

Abstract:
Part one of this month’s Q&A discusses transverse reinforcement requirements of Section 18.13.2.4 in ACI 318-19 and their relevance to foundation elements supporting structural steel frame systems. While part two focuses on Provision 19.2.1.3 in ACI 318-19 and its interpretation in regard to concrete mixtures that require strength testing at ages other than 28 days.




  