Title: Advances in X-Ray Computed Tomography for the Characterization of Cementitious Materials

Author(s): Jamie V. Clark, Tyler J. Deboodt, David A. Lange, Jason H. Ideker, and O. Burkan Isgor

Publication: Concrete International

Volume: 42

Issue: 9

Appears on pages(s): 30-36

Keywords: sample, phase, cellular, synchrotron

Date: 9/1/2020

Abstract:
X-ray computed tomography (XCT) is noninvasive and nondestructive. It produces three-dimensional digital reconstructions of samples, allowing for a comprehensive view of microstructure. The article discusses the use of XCT to examine cementitious materials. Three case studies are provided: characterization of cellular concrete microstructure, quantitative analysis of cement phases, and real-time investigation of an alkali-silica reaction.




  