Title: Monitoring Concrete Placements

Author(s):

Publication: Concrete International

Volume: 41

Issue: 12

Appears on pages(s): 42-43

Keywords: data, transmitter, thermocouple, curing

Date: 12/1/2019

Abstract:

MaturixTM, a concrete placement monitoring system, can be used to determine the temperature and strength of concrete placements. The system comprises type K or type A temperature sensors coupled to reusable, weatherproof wireless transmitters. After concrete is placed, the transmitters begin sending data that can be monitored using a mobile device or computer.




  