Withstanding Wear in Bulk Material Applications

ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

International Concrete Abstracts Portal

  


Title: Withstanding Wear in Bulk Material Applications

Author(s):

Publication: Concrete International

Volume: 41

Issue: 6

Appears on pages(s): 46-47

Keywords: liner, equipment, abrasion, plant

Date: 6/1/2019

Abstract:
Urethane liners can provide superior wear resistance for components in equipment used for aggregate production and handling. Urethane liner material is available in sheet form or in custom-molded shapes. Relative to conventional rubber liners, urethane liners provide a lower coefficient of friction, resulting in improved equipment cleanability between wet batches and enhancing productivity.




  

Please enter this 5 digit unlock code on the web page.