Title: Versatile, Swift, and True

Author(s): Hoskins, J.

Publication: Concrete International

Volume: 41

Issue: 6

Appears on pages(s): 48-50

Keywords: wall, construction, concrete, slab

Date: 6/1/2019

Abstract:
The VST stay-in-place formwork system is used in the construction of multistory residential, mixed-use, and commercial buildings in Europe and the United Kingdom. The formwork is used to construct cast-in-place, reinforced concrete load-bearing walls, floor slabs, columns, and stairs. Formwork assemblies are custom built for each project, and they are delivered with factory-installed reinforcement. The system minimizes construction waste and field labor.




  

Please enter this 5 digit unlock code on the web page.