Rehabilitation of Moderately Damaged Reinforced Concrete Buildings After June 27, 1998 Ceyhan Earthquake

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rehabilitation of Moderately Damaged Reinforced Concrete Buildings After June 27, 1998 Ceyhan Earthquake

Author(s): G. Ozcebe, H. Sucuoglu, M. 0. Sonuvar, and T. Gur

Publication: Symposium Paper

Volume: 193

Issue:

Appears on pages(s): 937-958

Keywords: capacity; concrete (reinforced); repair; strength

DOI: 10.14359/9969

Date: 8/1/2000

Abstract:
This paper reports on the interventions carried out by the Middle East Technical University faculty and staff on the moderately damaged 120 buildings in Ceyhan, Turkey after the June 27, 1998 earthquake. Discussion includes the organization ofthe intervention as well as its stages. Paper includes results of some recent research carried out at METU laboratories on infilling frames and detailed analytical evaluation of the strengthening scheme applied on the buildings.