Gravity Load-Designed Reinforced Concrete Buildings--Part II: Evaluation of Detailing Enhancements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Gravity Load-Designed Reinforced Concrete Buildings--Part II: Evaluation of Detailing Enhancements

Author(s): Sashi K. Kunnath, Garret Hoffmann, Andrei M. Reinhorn, and John B. Mander

Publication: Structural Journal

Volume: 92

Issue: 4

Appears on pages(s): 470-478

Keywords: buildings; confined concrete; costs; damage; joints (junctions); earthquake resistant structures; reinforced concrete; shear strength; structural analysis; Structural Research

DOI: 10.14359/996

Date: 7/1/1995

Abstract:
The seismic performance of a reinforced concrete (RC) building designed primarily for gravity loads was presented in the first part of this investigative study. Since the source of most of the structural damage is attributed to nonseismic details in the beam-column joint area, it was decided to examine the effects of improving these details in a marginal way, so that the seismic performance could be enhanced without resorting to a full seismic design. An extensive parametric study of the original buildings with refined detailing characteristics is carried out to ascertain effectiveness of the techniques to improve seismic resistance of gravity load-designed buildings. The important feature of the study is that the buildings are not redesigned for lateral forces, but only that detailing in critical regions is altered to achieve improved performance. This study may also be viewed indirectly as an inquiry into the effectiveness of retrofit strategies, should they be considered in real practice. The investigation also includes a cost evaluation of the various detailing schemes.