Development of Optical Fiber Sensor for Monitoring Concrete Performance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of Optical Fiber Sensor for Monitoring Concrete Performance

Author(s): H. Hamada, T. Yamaji, K. Hayakawa, and H. Yamashita

Publication: Symposium Paper

Volume: 193

Issue:

Appears on pages(s): 605-620

Keywords: concrete (structural); deterioration; sensor

DOI: 10.14359/9948

Date: 8/1/2000

Abstract:
In this study, two types of optical fiber sensors attached on the concrete surface, called a Straight-type sensor and Loop-type sensor were developed. Through bending tests of RC beam specimens, detailed data on beam deflection and optical performance of attached fiber were collected. Overall performance of the optical fiber sensor as a concrete performance monitor is discussed. Test procedures, test results and their discussions are summarized. Based on the experimental result, several conclusions were obtained. 1) The adhesion of epoxy resin to concrete surface is not lost until ultimate concrete failure. 2) The sensitivity of the Straight-type sensor is affected by the angle of concrete cracking and optical fiber intersection. 3) The distance between cracking location and looped circle of optical fiber affects the sensitivity of the Loop-type sensor. 4) Both for the straight type and the loop type, in order to develop a satisfactory level sensor, further research is strongly recommended.