Labcrete, Realcrete, and Hypocrete Where We can Expect the Next Major Durability Problems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Labcrete, Realcrete, and Hypocrete Where We can Expect the Next Major Durability Problems

Author(s): K. Newman

Publication: Symposium Paper

Volume: 100

Issue:

Appears on pages(s): 1259-1286

Keywords: alkali-aggregate reactions; concrete construction; concrete durability; construction materials: corrosion; deterioration; high-alumina cements; mix proportioning; siliceous aggregates; specifications; structural desiqn

DOI: 10.14359/9942

Date: 4/1/1987

Abstract:
This paper tries to draw lessons from major failures in the past two decades in the UK and gives a personal view as to why we still have problems in concrete today. Definitions are given of "Labcrete", "Realcrete" and "Hypocrete" and an examination is made of recent difficulties in the UK involving high-alumina cement, corrosion of reinforcing steel, alkali-silica reaction, and the definition of criteria for durability. A prediction is then made as to why and where further deterioration of concrete structures can be expected in the next 10 to 20 years. Finally, proposals are made for overcoming durability problems in the longer term; Above all there is a need to integrate our knowledge and understanding of the mechanisms of deterioration with concrete design, materials, methods of construction, and use.