City of Wichita Implements Pioneering Rehab Technologies

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: City of Wichita Implements Pioneering Rehab Technologies

Author(s): Karl J. Svaty, Jr., Monica Lane, Nabil F. Grace, and Jay Thomas

Publication: Concrete International

Volume: 22

Issue: 11

Appears on pages(s): 38-42

Keywords:

DOI:

Date: 11/1/2000

Abstract:
Planning for transportation needs involves many questions concerning aging bridges and their ability to carry ever-increasing traffic loads. For example, should a particular structure be closed to the detriment of traffic flow and nearby business activities, or is the bridge still in good structural condition? Could aggressive rehabilitation methods prolong the life of the structure, plus keep it open for use during that rehabilitation? The South Broadway Railroad Overpass in Wichita, Kan., is one case where the rehabilitation strategy worked extremely well.