Carbon Fiber Reinforced Concrete as an Intrinsically Smart Concrete for Damage Assessment during Static and Dynamic Loading

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Carbon Fiber Reinforced Concrete as an Intrinsically Smart Concrete for Damage Assessment during Static and Dynamic Loading

Author(s): Pu-Woei Chen and D. D. L. Chung

Publication: Materials Journal

Volume: 93

Issue: 4

Appears on pages(s): 341-350

Keywords: carbon; concretes; damage; dynamic loads; electrical resis-tance; fibers.

DOI: 10.14359/9820

Date: 7/1/1996

Abstract:
Concrete containing short carbon fibers (in amounts as small as 0.2 vol-ume- percent) was found to be an intrinsically smart concrete that can sense elastic deformation, inelastic deformation, and fracture. The signal provided is the change in electrical resistance, which is reversible for elastic deformation and irreversible for inelastic deformation and fracture. The presence of electrically conducting short fibers is necessary for the concrete to sense elastic or inelastic deformation, but the sensing of fracture does not require fibers. The fibers serve to bridge the cracks and provide a conduction path. The resistance increase is due to conducting fiber pullout in the elastic regime, conducting fiber breakage in the inelastic regime, and crack propagation at fracture. Applications include real-time damage assessment and dynamic load monitoring.