Mechanisms of Delayed Ettringite Formation in Portland Cement Systems

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanisms of Delayed Ettringite Formation in Portland Cement Systems

Author(s): Yan Fu and James J. Beaudoin

Publication: Materials Journal

Volume: 93

Issue: 4

Appears on pages(s): 327-333

Keywords: cement; ettringite; expansion; gypsum; precast concrete; temperature.

DOI: 10.14359/9818

Date: 7/1/1996

Abstract:
Sulfate adsorption from internal sources in systems containing gypsum and C-S-H gel derived from either hydrating C3S or portland cement was studied with respect to delayed ettringite formation. The influence of C3A addi-tion on sulfate desorption was also investigated. Research indicates that C-S-H gel will adsorb sulfate faster at elevated temperatures, resulting in quick depletion of the gypsum phase in C-S-H-gypsum mixes. The critical temperature for sulfate adsorption by C-S-H gel is above 65 C. Sulfate adsorbed at high temperatures is desorbed more slowly than that adsorbed at normal temperatures. The slower release of sulfate from an internal sulfate source may be a critical condition for delayed ettringite formation in high-temperature-cured portland cement paste. Two competitive reactions in terms of gypsum consumption are discussed. These involve both C-S-H gel and the hydrated calcium aluminates. Further evidence in support of a hypothesis for preferred nucleation of delayed ettringite in cracks in portland cement paste is presented. Results presented indicate that the reactants for delayed ettringite formation in cracks can come from sources away from the cracks. Diffusion of reactant ions through concrete pore solution appears to be a key element of the process responsible for initiation of delayed ettringite nucleation in cracks.