Abstract of: Guide for the Use of Silica Fume in Concrete (ACI 234R)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Abstract of: Guide for the Use of Silica Fume in Concrete (ACI 234R)

Author(s): ACI Committee 234

Publication: Materials Journal

Volume: 92

Issue: 4

Appears on pages(s): 437-440

Keywords: alkali-silica reactions; compressive strength; durability; corrosion resistance; curing; drying shrinkage; finishes; fresh concretes; hardened concretes; high-strength concretes; microstructure; permeability; placing; silica fume; specifications; Material

DOI: 10.14359/978

Date: 7/1/1995

Abstract:
This report describes the physical and chemical properties of silica fume; how silica fume interacts with portland cement; the effects of silica fume on the properties of fresh and hardened concrete; recent typical applications of silica-fume concrete; how silica-fume concrete is proportioned, specified, and handled in the field; and areas where additional research is needed.