Abstract of: State-of-the-Art Report on Roller Compacted Concrete Pavements

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Abstract of: State-of-the-Art Report on Roller Compacted Concrete Pavements

Author(s): ACI Committee 325

Publication: Materials Journal

Volume: 91

Issue: 5

Appears on pages(s): 509-510

Keywords: aggregates; cements; compaction; concrete construction; con-crete durability; concrete pavements; consolidation; curing; construction joints; density; mixing; placing; portland cement; roller compacted con-crete, strength.

DOI: 10.14359/9760

Date: 9/1/1994

Abstract:
This report covers the present state of the art for roller compacted concrete pavements. It contains information on applications, material properties, mix proportioning, *design, construction, and quality control procedures. Roller compacted concrete use for pavements is relatively recent and the technology is still evolving. The pavement consists of a relatively stiff mixture of aggregate, cementitious materials, and water; that is compacted by rollers and hardened into concrete.