Strength of Masonry Subjected to Combined Actions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strength of Masonry Subjected to Combined Actions

Author(s): Nebojsa Mojsilovic and Peter Marti

Publication: Structural Journal

Volume: 94

Issue: 6

Appears on pages(s): 633-642

Keywords: bending; limit analysis; loads (forces); masonry; strength; struc-tural design; tests; walls.

DOI: 10.14359/9723

Date: 11/1/1997

Abstract:
A sandwich model is presented to predict the strength of masonry wall elements subjected to combined in-plane forces and moments, The validity of the model is demonstrated by comparisons with eighteen large-scale tests on clay brick and calcium-silicate block walls. While the experimental verification has been limited to clay brick and calcium-silicate block masonry, the sandwich model is also applicable to concrete block masonry.