Title: Abstract of: State-of-the-Art-Report on Flber Reinforced Plastic (FRP) for Concrete Structures

Author(s): ACI Committee 440

Publication: Structural Journal

Volume: 92

Issue: 5

Appears on pages(s): 627-628

Keywords: composite materials; concrete; concrete construction; design; external reinforcement; fiber reinforced plastic (FRP); fibers; mechanical properties; polymer

DOI: 10.14359/9658

Date: 11/1/1995

Abstract:
The use of FRP as reinforcement for concrete structures has been growing rapidly in recent years. This state-of-the-art report summarizes the current state of knowledge on these materials. In addition to the material properties of the constituents, i.e., resins and fibers, design philosophies for reinforced and prestressed elements are discussed. When the available data warrant flexure, shear, and bond behavior; and serviceability of the members has been examined. Strengthening of existing structures with FRPs and field applications of these materials are also presented.