Shear Strength Prediction for Deep Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength Prediction for Deep Beams

Author(s): Shyh-Jiann Hwang, Wen-Yao Lu, and Hung-Jen Lee

Publication: Structural Journal

Volume: 97

Issue: 3

Appears on pages(s): 367-376

Keywords: deep beams; reinforced concrete; shear strength.

DOI: 10.14359/9624

Date: 5/1/2000

Abstract:
a softened strut-and-tie model for determining the shear strengths of deep beams is proposed in this paper. The proposed model originates from the strut-and-tie concept and satisfies equilibrium, compatibility, and constitutive laws of cracked reinforced concrete. The shear strength prediction of the proposed model and the empirical shear strength prediction s of the proposed model and the empirical formulas of the ACI 318-95 Code compared with the collected experimental data of 123 deep beams. The comparison show that experimental data of 123 deep beams. The comparison shows that the performance of the softened strut and tie model is better that the ACI Code approach for all the parameters under comparison. The parameters reviewed include the ratios of horizontal and vertical reinforcement, concrete strength, and the shear span depth ratio. The softened strut and tie model can be further developed to improve the current deep beam design procedures by incorporating the actual shear resisting mechanisms in predicting shear strength supply of deep beams.


ALSO AVAILABLE IN: