Industrial Flooring with Steel Fiber Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Industrial Flooring with Steel Fiber Concrete

Author(s): Mark P. Vandenberghe, Dirk E. Nemegeer

Publication: Concrete International

Volume: 7

Issue: 3

Appears on pages(s): 54-57

Keywords: fatigue (materials); fiber reinforced concretes; flexural strength; floors; heavy-duty floors; industrial buildings; metal fibers; pumped concrete; warehouses

DOI:

Date: 3/1/1985

Abstract:
The use of steel fibers in the reinforcement of industrial floors has become a widely accepted practice in Europe. The use of the fibers in a major United States project in Holland is likely to offer the American reader an instructive example.